the root bead welded
With the 6.4 mm steel plate,only the root bead welded over the ceramic backing was evaluated.With the 15.8 mm steel plate,a
multipass welded joint was made.After welding,the welded joints were submitted to visual inspection,dye penetrant,
macrograph,Vickers microhardness,optical microscopy,bending and tensile testing and chemical analysis using non-
destructive test.