Martensitic steels--2
Particularly with complicated structures, it is usual to butter the joint faces with an
austenitic filler metal. Each part of the workpiece is treated separately and heat-treated.
The austenitic layer is built up to a sufficient thickness to ensure that no metallurgical
change occurs in the base material when the final weld is made.
.